Plastic recycling machine for film scrap pelletizing to solve screen clogging

How to Solve Frequent Screen Clogging Problems in Film Scrap Pelletizing

 

The root causes of frequent screen clogging when pelletizing recycled film scrap are high impurity content, high moisture levels, and uneven plasticization. Solving this issue requires a combination of “upstream pre-treatment,” “core screen changer system upgrades,” and “fine-tuning of process parameters.” Specific solutions are outlined below:

 

 

1、Upstream Pre-treatment: Reducing Impurities at the Source

 

Strengthened Washing and Dewatering: Recycled film scrap (especially agricultural and packaging films) often contains over 20% moisture and sediment. It is essential to equip the washing line with high-efficiency friction washers and centrifugal dewatering machines to keep moisture content below 15%. This prevents moisture vaporization during extrusion, which causes melt pressure fluctuations and impurity agglomeration.

Add Pre-screening: Install magnetic separation devices before the shredded material enters the extruder to remove metal debris early, thereby reducing the load on the downstream melt filtration system.

 

 

2、Core Equipment Upgrades: Screen Changer and Filter Configuration

 

① Equip with a Continuous Screen Changer: Processing recycled material requires a screen changer; a dual-plate, dual-station continuous screen changer is the preferred choice. Its key advantage is that the two filtration chambers operate in parallel; when one side becomes clogged, the hydraulic system automatically switches to the other side (which holds a pre-heated, clean screen). This allows for screen changes without stopping the machine, keeps pressure fluctuations within 1–3%, and ensures more stable extrusion.

 

② Increase Filtration Area: Excessive screen-changing frequency is often caused by an undersized filtration area. When dealing with recycled material carrying a high impurity load, a sufficiently large filtration area must be selected to extend the service life of each screen.

 

③ Adopt a Gradient Filter Combination: Avoid relying on a single layer of high-mesh screen to handle the entire load. A multi-layer combination—such as 40-mesh + 80-mesh + 120-mesh—is recommended, consisting of coarse filtration, fine filtration, and a support layer. The coarse filter traps large particles, the fine filter ensures purity, and the support mesh prevents deformation under high pressure. This gradient filtration approach significantly distributes the load and extends screen life by more than 30%.

Film scrap pelletizing screen clogging troubleshooting

 

3、Fine-tuning Process Parameters: Optimizing Melt Flow

 

① Appropriately increase die temperature: Excessively low temperatures in the extruder or die can lead to poor plasticization and high melt viscosity, making it easier for impurities to adhere to the walls and cause blockages. Raising the temperature of the final barrel section and the die plate (typically to 10°C above the bubble channel temperature) can significantly reduce melt viscosity and enhance the melt’s ability to scour and self-clean the die orifices.

 

② Temperature reduction during shutdown: When a prolonged production stoppage is anticipated, temperatures across all processing zones must be lowered immediately upon shutdown to prevent the thermal degradation and carbonization of residual material caused by sustained high temperatures.

 

In conclusion, eliminating screen clogging in film scrap pelletizing relies on systematic optimization from raw material pretreatment, equipment configuration to production process adjustment, which can effectively reduce screen replacement frequency, improve production efficiency and lower operational costs.
If you encounter persistent screen clogging problems or have personalized demands for equipment upgrading and process parameter debugging in actual production, feel free to consult our professional engineering team. We provide one-to-one targeted technical guidance and customized solutions to help you solve production bottlenecks thoroughly and achieve stable and efficient pelletizing production.
Request a Quote
All products are guaranteed for 12 months!